Description

120WJ is a Linear Low Density Polyethylene TNPP free grade suitable for general purpose packaging. Films produced using these resins gives good tensile properties, impact strength and excellent optical properties. 120WJ contains slip and antiblock additive.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

0.92 g/cm³

Show Material materials with Density of 0.92 g/cm³

ASTM D1505

Thermal

PropertyValueComment

Vicat softening temperature

100 °C

Show Material materials with Vicat softening temperature of 100 °C

ASTM D1525

Optical

PropertyValueComment

Haze

10 %

Show Material materials with Haze of 10 %

ASTM D1003

Technological properties

Property
Application areas

Stretch film,Shrink film,Blown film,General purpose film