SABIC® LLDPE 128CNJ

Want to keep this datasheet? Save it now in your required format

Description

128CNJ is a Linear Low Density Polyethylene natural resin designed for extrusion applications. This grade is combining stiffness, toughness, high melt strength with an excellent processability due to its broad molecular weight distribution. It is TNPP free and contains an optimized level of stabilizers and does not contain any slip or anti-block additives.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

0.93 g/cm³

Show Material materials with Density of 0.93 g/cm³

ASTM D1505

Mechanical

PropertyTemperatureValueComment

Elongation

23.0 °C

850 %

Show Material materials with Elongation of 850 %

ASTM D638

Elongation at yield

23.0 °C

12 %

Show Material materials with Elongation at yield of 12 %

ISO 527-1/-2

Hardness, Shore D

23.0 °C

48 [-]

Show Material materials with Hardness, Shore D of 48 [-]

ASTM D2240

Tensile strength

23.0 °C

25 MPa

Show Material materials with Tensile strength of 25 MPa

ASTM D638

Yield strength

23.0 °C

14 MPa

Show Material materials with Yield strength of 14 MPa

ASTM D638

Electrical

PropertyTemperatureValueComment

Dielectric constant

23.0 °C

2.2 [-]

Show Material materials with Dielectric constant of 2.2 [-]

ASTM D 150 | at 1 KHz

Electrical resistivity

23.0 °C

0.01 Ω·m

Show Material materials with Electrical resistivity of 0.01 Ω·m

ASTM D 257 | at 500V

Technological properties

Property
Application areas

Electrical,Wire & cable