SABIC® LDPE 2005EC

Want to keep this datasheet? Save it now in your required format

Description

SABIC® LDPE 2005EC is the first commercially proven tubular LDPE grade for extrusion coating. The product gives a good combination of processing and end-performance properties. SABIC® LDPE 2005EC can be used on low and (very) high line speed extrusion coating and lamination processes. Due to its excellent draw down performance and good adhesion, very thin coating layers can be applied on the substrate. Application SABIC® LDPE2005EC is typically used in extrusion coating and lamination applications, such as liquid packaging, food packaging and building & construction. Typical substrates for coating or lamination are paper, board, aluminum, PET or PA. Properties Mechanical properties determined on compression moulded specimen (2 mm thick) at test speed of 50 mm/min. Film properties have been measured at film of 25 µm, produced on lab scale equipment. Water vapour permeability at 38 °C and 90 % RH per 24 h. Oxygen permeability at 23 °C and 0 % RH per 24 h. This product is not intended for and must not be used in any pharmaceutical/medical applications.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

0.92 g/cm³

Show Material materials with Density of 0.92 g/cm³

ASTM D1505

Mechanical

PropertyTemperatureValueComment

Tear strength

23.0 °C

45 kN/m

Show Material materials with Tear strength of 45 kN/m

ISO 6383-2

Tear strength, transverse

23.0 °C

45 kN/m

Show Material materials with Tear strength, transverse of 45 kN/m

ISO 6383-2

Technological properties

Property
Application areas

Extrusion coating and lamination applications (liquid packaging, food packaging and building & construction)