SABIC® LDPE 2101N0W

Want to keep this datasheet? Save it now in your required format

Description

SABIC® LDPE 2101N0W is a grade with good toughness and biaxial shrink properties. The material contains no additives, has a low energy consumption during processing and a good draw down ability. Application SABIC® LDPE 2101N0W is typically used for thin shrink film. SABIC® LDPE 2101N0W can typically be used for food applications due to very low migration levels. Film properties Film properties have been measured at 50 μm film with a BUR of 3. The film has been produced on Kiefel IBC film blown line at 200 kg/h. Die size 200 mm, die gap 0.8 mm. This product is not intended for and must not be used in any pharmaceutical/medical applications.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Coefficient of friction

1 [-]

Show Material materials with Coefficient of friction of 1 [-]

ASTM D1894

Density

23.0 °C

0.92 g/cm³

Show Material materials with Density of 0.92 g/cm³

ASTM D1505

Mechanical

PropertyTemperatureValueComment

Tear strength

23.0 °C

40 kN/m

Show Material materials with Tear strength of 40 kN/m

ISO 6383-2

Tear strength, transverse

23.0 °C

30 kN/m

Show Material materials with Tear strength, transverse of 30 kN/m

ISO 6383-2

Optical

PropertyValueComment

Haze

9 %

Show Material materials with Haze of 9 %

ASTM D1003

Technological properties

Property
Application areas

It is used for food applications (thin shrink film) due to very low migration levels.