SABIC® LDPE 2102N3W

Want to keep this datasheet? Save it now in your required format

Description

SABIC® LDPE 2102N3W is a general purpose grade with a high level of anti block and slip agent. This grade offers good optical properties and a very good draw down ability. Application SABIC® LDPE 2102N3W is typically used for packaging films for food and industrial goods and for lamination films. This grade is typically used when high draw down is required The usual melt-2 film thickness can be reduced by 10-40%, maintaining an adequate CoF level. SABIC® LDPE 2102N3W can typically be used for food applications due to very low migration levels. Film properties Film properties have been measured at film of 25 μm with a BUR of 3. The film has been produced on Kiefel IBC blown film line with 200 kg/h. Die size 200 mm, die gap 0.8 mm. This product is not intended for and must not be used in any pharmaceutical/medical applications.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Coefficient of friction

0.2 [-]

Show Material materials with Coefficient of friction of 0.2 [-]

ASTM D1894

Density

23.0 °C

0.92 g/cm³

Show Material materials with Density of 0.92 g/cm³

ASTM D1505

Mechanical

PropertyTemperatureValueComment

Tear strength

23.0 °C

50 kN/m

Show Material materials with Tear strength of 50 kN/m

ISO 6383-2

Tear strength, transverse

23.0 °C

20 kN/m

Show Material materials with Tear strength, transverse of 20 kN/m

ISO 6383-2

Optical

PropertyValueComment

Haze

12 %

Show Material materials with Haze of 12 %

ASTM D1003

Technological properties

Property
Application areas

Packaging films for food and industrial goods and for lamination films