SABIC® LDPE 2102X3

Want to keep this datasheet? Save it now in your required format

Description

SABIC® LDPE 2102X3 is typically used in foam applications. Application SABIC® LDPE 2102X3 can be typically used for all types of foam, produced with chemical blowing agents or physical gases, X-linked and non X-linked. This product is not intended for and must not be used in any pharmaceutical/medical applications.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

0.92 g/cm³

Show Material materials with Density of 0.92 g/cm³

ASTM D1505

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

0.25 GPa

Show Material materials with Elastic modulus of 0.25 GPa

SABIC method

Hardness, Shore D

23.0 °C

45 [-]

Show Material materials with Hardness, Shore D of 45 [-]

ISO 868

Technological properties

Property
Application areas

It is used for all types of foam, produced with chemical blowing agents or physical gases, X-linked and non X-linked.