SABIC® LLDPE 218BE is a butene linear low density polyethylene resin with an additive package typically designed for a broader range of food applications (TNPP free). The good thermal stability allows to use the resin in critical extrusion processing conditions. Application SABIC® LLDPE 218BE is typically used for food applications (lamination film, barrier film) but can also be used in industrial packaging and as blending partner with other SABIC® PE resins in both blown and cast film applications. This product is not intended for and must not be used in any pharmaceutical/medical applications.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

0.92 g/cm³

Show Material materials with Density of 0.92 g/cm³

ASTM D1505

Mechanical

PropertyTemperatureValueComment

Hardness, Shore D

23.0 °C

48 [-]

Show Material materials with Hardness, Shore D of 48 [-]

ISO 868

Tear strength, transverse

23.0 °C

185 kN/m

Show Material materials with Tear strength, transverse of 185 kN/m

ISO 6383-2

Electrical

PropertyTemperatureValueComment

Dielectric constant

23.0 °C

2.17 [-]

Show Material materials with Dielectric constant of 2.17 [-]

ASTM D150 | at 60 Hz

Dielectric strength

23.0 °C

55 kV/mm

Show Material materials with Dielectric strength of 55 kV/mm

ASTM D149 | at 500 V/sec

Dissipation factor

23.0 °C

1000 [-]

Show Material materials with Dissipation factor of 1000 [-]

ASTM D150 | at 60 Hz

Electrical resistivity

23.0 °C

5.00E+13 Ω·m

Show Material materials with Electrical resistivity of 5.00E+13 Ω·m

ASTM D257

Optical

PropertyValueComment

Haze

1.2 %

Show Material materials with Haze of 1.2 %

ASTM D1003

Technological properties

Property
Application areas

It is typically used for food applications (lamination film, barrier film) but can also be used in industrial packaging and as blending partner with other SABIC® PE resins in both blown and cast film applications.