SABIC® LLDPE 218NJ

Want to keep this datasheet? Save it now in your required format

Description

218NJ is a butene Linear Low Density Polyethylene TNPP free grade suitable for general‐purpose packaging. It is easy to process giving good tensile properties, impact strength and optical properties. 218NJ contains no slip and no antiblock additives.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

0.92 g/cm³

Show Material materials with Density of 0.92 g/cm³

ASTM D1505

Thermal

PropertyValueComment

Vicat softening temperature

98 °C

Show Material materials with Vicat softening temperature of 98 °C

ASTM D1525

Optical

PropertyValueComment

Haze

13 %

Show Material materials with Haze of 13 %

ASTM D1003

Technological properties

Property
Application areas

Blown film,General purpose film,Lamination film