SABIC® LLDPE 220WT

Want to keep this datasheet? Save it now in your required format

Description

SABIC® 220WT is an ethylene-butene copolymer designed for blown film application. It has excellent stiffness, puncture resistance, high tensile strength, High clarity and high gloss. 220WT contains high slip and high antiblock.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

0.92 g/cm³

Show Material materials with Density of 0.92 g/cm³

ASTM D1505

Optical

PropertyValueComment

Haze

13 %

Show Material materials with Haze of 13 %

ASTM D1003

Technological properties

Property
Application areas

Stretch film,Blown film,Lamination film