SABIC® LDPE 2402H0

Want to keep this datasheet? Save it now in your required format

Description

SABIC® LDPE 2402H0 is a blown film grade which has a very broad processing window and an excellent draw down ability. The films are characterized by very good mechanical and optical properties. The grade contains no additives. Application SABIC® LDPE 2402H0 is typically used for thin film applications where enhanced stiffness is required, such as thin shrink films, food packaging films, bags and pouches. Film properties Film properties have been measured at film of 25 μm with a BUR of 3. The film has been produced on Kiefel IBC blown film line with 200 kg/h. Die size 200 mm, die gap 0.8 mm. This product is not intended for and must not be used in any pharmaceutical/medical applications.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Coefficient of friction

1 [-]

Show Material materials with Coefficient of friction of 1 [-]

ASTM D1894

Density

23.0 °C

0.92 g/cm³

Show Material materials with Density of 0.92 g/cm³

ASTM D1505

Mechanical

PropertyTemperatureValueComment

Tear strength

23.0 °C

80 kN/m

Show Material materials with Tear strength of 80 kN/m

ISO 6383-2

Tear strength, transverse

23.0 °C

35 kN/m

Show Material materials with Tear strength, transverse of 35 kN/m

ISO 6383-2

Optical

PropertyValueComment

Haze

7 %

Show Material materials with Haze of 7 %

ASTM D1003

Technological properties

Property
Application areas

Thin shrink films, food packaging films, bags and pouches