SABIC® LDPE 2404H4

Want to keep this datasheet? Save it now in your required format

Description

SABIC® LDPE 2404H4 is a grade with a high level of anti block and slip agent. The grade has a very good draw down ability. Typically films produced from this grade are stiff, have very good optical properties, low CoF and no blocking. Application SABIC® LDPE 2404H4 is typically used for stiffer thin films for textile packaging. Film properties Film properties have been measured at film of 25 μm with a BUR of 3. The film has been produced on Kiefel IBC blown film line with 200 kg/h. Die size 200 mm, die gap 0.8 mm. This product is not intended for and must not be used in any pharmaceutical/medical applications.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Coefficient of friction

0.2 [-]

Show Material materials with Coefficient of friction of 0.2 [-]

ASTM D1894

Density

23.0 °C

0.93 g/cm³

Show Material materials with Density of 0.93 g/cm³

ASTM D1505

Mechanical

PropertyTemperatureValueComment

Tear strength

23.0 °C

90 kN/m

Show Material materials with Tear strength of 90 kN/m

ISO 6383-2

Tear strength, transverse

23.0 °C

30 kN/m

Show Material materials with Tear strength, transverse of 30 kN/m

ISO 6383-2

Optical

PropertyValueComment

Haze

11 %

Show Material materials with Haze of 11 %

ASTM D1003

Technological properties

Property
Application areas

Stiffer thin films for textile packaging