Description

SABIC® LDPE 2602H0W is a grade with very good optical properties. The grade contains no additives, has an increased density and shows a good draw down ability. The films are characterized by good mechanical properties. Application SABIC® LDPE 2602H0W is typically used for applications where enhanced stiffness is required. SABIC® LDPE 2602H0W can typically be used for food applications due to very low migration levels. This product is not intended for and must not be used in any pharmaceutical/medical applications.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

0.93 g/cm³

Show Material materials with Density of 0.93 g/cm³

ASTM D1505

Mechanical

PropertyTemperatureValueComment

Tear strength

23.0 °C

90 kN/m

Show Material materials with Tear strength of 90 kN/m

ISO 6383-2

Tear strength, transverse

23.0 °C

40 kN/m

Show Material materials with Tear strength, transverse of 40 kN/m

ISO 6383-2

Optical

PropertyValueComment

Haze

6 %

Show Material materials with Haze of 6 %

ASTM D1003

Technological properties

Property
Application areas

General purpose film,Lamination film