SABIC® POM 30RE

Want to keep this datasheet? Save it now in your required format

Description

SABIC® POM 30RE is a special grade for Rods and Extrusion sheet applications free of center porosity in large diameter and thickness.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.41 g/cm³

Show Material materials with Density of 1.41 g/cm³

ISO 1183

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

2.4 GPa

Show Material materials with Elastic modulus of 2.4 GPa

ISO 527-2 1A | 1mm/min

Elongation at yield

23.0 °C

11 %

Show Material materials with Elongation at yield of 11 %

ISO 527-2 1A | 50mm/min

Flexural modulus

23.0 °C

2.5 GPa

Show Material materials with Flexural modulus of 2.5 GPa

ISO 178

Impact strength, Charpy notched

23.0 °C

8.5 kJ/m²

Show Material materials with Impact strength, Charpy notched of 8.5 kJ/m²

ISO 179/1eA

Yield strength

23.0 °C

61 MPa

Show Material materials with Yield strength of 61 MPa

ISO 527-2 1A | 50 mm/min

Thermal

PropertyValueComment

Heat deflection temperature, 1.80 MPa

91 °C

Show Material materials with Heat deflection temperature, 1.80 MPa of 91 °C

ISO 75-1&2 | 1.8 MPa

Melting point

163 °C

Show Material materials with Melting point of 163 °C

ISO 11357-1/-3

Rheological Properties

PropertyValueComment

Melt volume-flow rate

2.5 cm³/10min

Show Material materials with Melt volume-flow rate of 2.5 cm³/10min

ISO 1133

Technological properties

Property
Application areas

Automotive