Description

SABIC® LLDPE318B is a standard C4-LLDPE grade with a relatively low melt flow rate. SABIC® LLDPE318B is a general grade, typically used for low filled or additive masterbatches in film and blow moulding applications(e.g. slip agents, anti fog agents, anti static agents, thermal stabilizers). This product is not intended for and must not be used in any pharmaceutical/medical applications.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

0.92 g/cm³

Show Material materials with Density of 0.92 g/cm³

ASTM D1505

Mechanical

PropertyTemperatureValueComment

Hardness, Shore D

23.0 °C

48 [-]

Show Material materials with Hardness, Shore D of 48 [-]

ISO 868

Tear strength, transverse

23.0 °C

140 kN/m

Show Material materials with Tear strength, transverse of 140 kN/m

ISO 6383-2

Electrical

PropertyTemperatureValueComment

Dielectric constant

23.0 °C

2.2 [-]

Show Material materials with Dielectric constant of 2.2 [-]

ASTM D150 | at 60 Hz

Dissipation factor

23.0 °C

5E-4 [-]

Show Material materials with Dissipation factor of 5E-4 [-]

ASTM D150 | at 60 Hz

Electrical resistivity

23.0 °C

8.50E+13 Ω·m

Show Material materials with Electrical resistivity of 8.50E+13 Ω·m

ASTM D257

Optical

PropertyValueComment

Haze

2.1 %

Show Material materials with Haze of 2.1 %

ASTM D1003

Technological properties

Property
Application areas

Typically used for low filled or additive masterbatches in film and blow moulding applications(e.g. slip agents, anti fog agents, anti static agents, thermal stabilizers).