SABIC® LLDPE 324CE

Want to keep this datasheet? Save it now in your required format

Description

SABIC® LLDPE 324CE is a Linear Low Density Polyethylene natural resin typically used for wire and cable applications. SABIC® LLDPE 324CE contains a low level of antioxidants and does not contain any antiblock and/or slip agents. It also exhibits good Environmental Stress Crack Resistance (ESCR). Sufficient Cu-inhibitor should be added to meet specific ageing requirements. For jacketing applications, addition of Carbon Black or UV stabilizer is required. Applications - Telecommunication and Power cable (LV, MV, HV) jacketing. - Halogen-free flame retardant (HFFR) compounds. - One-step or two-steps silane crosslinkable for cable insulation. This product is not intended for and must not be used in any pharmaceutical/medical applications. Mechanical and electrical properties. Test specimens were prepared by compression moulding according to ASTM D 4703.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

0.92 g/cm³

Show Material materials with Density of 0.92 g/cm³

ASTM D1505

Mechanical

PropertyTemperatureValueComment

Hardness, Shore D

23.0 °C

53 [-]

Show Material materials with Hardness, Shore D of 53 [-]

ISO 868

Electrical

PropertyTemperatureValueComment

Dielectric constant

23.0 °C

2.2 [-]

Show Material materials with Dielectric constant of 2.2 [-]

ASTM D150 | at 60 Hz

Dissipation factor

23.0 °C

5E-4 [-]

Show Material materials with Dissipation factor of 5E-4 [-]

ASTM D150 | at 60 Hz

Electrical resistivity

23.0 °C

8.50E+13 Ω·m

Show Material materials with Electrical resistivity of 8.50E+13 Ω·m

ASTM D257

Technological properties

Property
Application areas

It is used for wire and cable applications (telecommunication and power cable (LV, MV, HV) jacketing, halogen-free flame retardant (HFFR) compounds, one-step or two-steps silane crosslinkable for cable insulation).