Description

324CNJ is a Linear Low Density Polyethylene TNPP free grade designed for wire and cable applications. It contains low level of antioxidants and does not contain any slip and antiblock additives. Sufficient antioxidant and Cu-inhibitor should be added to meet specific ageing requirements. For jacketing applications, addition of Carbon Black or UV stabilizer is required.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

0.92 g/cm³

Show Material materials with Density of 0.92 g/cm³

ASTM D1505

Mechanical

PropertyTemperatureValueComment

Hardness, Shore D

23.0 °C

53 [-]

Show Material materials with Hardness, Shore D of 53 [-]

ISO 868

Thermal

PropertyValueComment

Melting point

121 °C

Show Material materials with Melting point of 121 °C

SABIC method

Electrical

PropertyTemperatureValueComment

Dielectric constant

23.0 °C

2.2 [-]

Show Material materials with Dielectric constant of 2.2 [-]

ASTM D150 | at 60 Hz

Dielectric strength

23.0 °C

55 kV/mm

Show Material materials with Dielectric strength of 55 kV/mm

ASTM D149 | at 500 V/sec

Dissipation factor

23.0 °C

5E-4 [-]

Show Material materials with Dissipation factor of 5E-4 [-]

ASTM D150 | at 60 Hz

Electrical resistivity

23.0 °C

8.50E+13 Ω·m

Show Material materials with Electrical resistivity of 8.50E+13 Ω·m

ASTM D257

Technological properties

Property
Application areas

Wire & cable