LEXAN™ FR Resins 3412R

Want to keep this datasheet? Save it now in your required format

Description

20% GR, provides improved mechanical properties and UL94 V-1 rated at 0.058". Internal mold release added.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.35 g/cm³

Show Material materials with Density of 1.35 g/cm³

ISO 1183

Water absorption

23.0 °C

0.12 %

Show Material materials with Water absorption of 0.12 %

ISO 62 | 23°C, 50% RH

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

6 GPa

Show Material materials with Elastic modulus of 6 GPa

ISO 527 | 1 mm/min

Elongation

23.0 °C

2 %

Show Material materials with Elongation of 2 %

ISO 527 | 5 mm/min

Flexural modulus

23.0 °C

5.5 GPa

Show Material materials with Flexural modulus of 5.5 GPa

ISO 178 | 2 mm/min

Flexural strength

23.0 °C

120 MPa

Show Material materials with Flexural strength of 120 MPa

ISO 178

Hardness, Ball Indentation

23.0 °C

125 MPa

Show Material materials with Hardness, Ball Indentation of 125 MPa

ISO 2039-1

Impact strength, Charpy notched

23.0 °C

9 kJ/m²

Show Material materials with Impact strength, Charpy notched of 9 kJ/m²

ISO 179/2C

Impact strength, Charpy unnotched

-30.0 °C

40 kJ/m²

Show Material materials with Impact strength, Charpy unnotched of 40 kJ/m²

ISO 179/1eU

23.0 °C

40 kJ/m²

Show Material materials with Impact strength, Charpy unnotched of 40 kJ/m²

ISO 179/1eU

Impact strength, Izod notched

-30.0 °C

6 kJ/m²

Show Material materials with Impact strength, Izod notched of 6 kJ/m²

ISO 180/1A

23.0 °C

7 kJ/m²

Show Material materials with Impact strength, Izod notched of 7 kJ/m²

ISO 180/1A

Unlock all property charts

Impact strength, Izod unnotched

-30.0 °C

35 kJ/m²

Show Material materials with Impact strength, Izod unnotched of 35 kJ/m²

ISO 180/1U

23.0 °C

35 kJ/m²

Show Material materials with Impact strength, Izod unnotched of 35 kJ/m²

ISO 180/1U

Unlock all property charts

Tensile strength

23.0 °C

90 MPa

Show Material materials with Tensile strength of 90 MPa

ISO 527 | 5 mm/min

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

3E-5 1/K

Show Material materials with Coefficient of thermal expansion of 3E-5 1/K

ISO 11359-2 | -23°C to 80°C

Heat deflection temperature, 1.80 MPa

139 °C

Show Material materials with Heat deflection temperature, 1.80 MPa of 139 °C

ISO 75/Ae | 1.8 MPa

Relative temperature index, electrical

130 °C

Show Material materials with Relative temperature index, electrical of 130 °C

UL 746B

Relative temperature index, mechanical impact

125 °C

Show Material materials with Relative temperature index, mechanical impact of 125 °C

UL 746B

Relative temperature index, mechanical strength

130 °C

Show Material materials with Relative temperature index, mechanical strength of 130 °C

UL 746B

Thermal conductivity

23.0 °C

0.22 W/(m·K)

Show Material materials with Thermal conductivity of 0.22 W/(m·K)

ISO 8302

Vicat softening temperature

145 °C

Show Material materials with Vicat softening temperature of 145 °C

ISO 306 | Rate B/120

Flammability

UL Recognized, 94V-0 Flame Class Rating | 1.5mm | UL 94

Electrical

PropertyTemperatureValueComment

Comparative tracking index

23.0 °C

150 V

Show Material materials with Comparative tracking index of 150 V

IEC 60112

Dielectric constant

23.0 °C

3 [-]

Show Material materials with Dielectric constant of 3 [-]

IEC 60250 | at 50/60 Hz

Dielectric strength

23.0 °C

16 kV/mm

Show Material materials with Dielectric strength of 16 kV/mm

IEC 60243-1 | in oil, 3.2 mm

Dissipation factor

23.0 °C

0.01 [-]

Show Material materials with Dissipation factor of 0.01 [-]

IEC 60250 | at 1 MHz

Rheological Properties

PropertyTemperatureValueComment

Melt volume-flow rate

6 cm³/10min

Show Material materials with Melt volume-flow rate of 6 cm³/10min

ISO 1133 | 300°C/1.2 kg

Shrinkage

23.0 °C

0.2 - 0.5 %

Show Material materials with Shrinkage of 0.2 - 0.5 %

SABIC method

Technological properties

Property
Application areas

Aerospace,Air Cabin Interiors,Amusement Machine,ATM/Ticket Machine,Audio,Auto Aftermarket,Building Accessory,Building Element,Circuit Protection,Coffee Maker/Espresso Machine,Data Management,Data Transfer,Displays,Document Handling,Door Handle,Electronic Components,Enclosure/Housing/Cover,Enclosures,Energy Management,Exercise Equipment,Fixture Bath/Shower,Food Processor,Heavy Vehicles,Lab Ware and Clinical Diagnostics,Lawn/Garden,LED Lighting,Medical Device,Medical Facility Infrastructure,Meter Water,Monitoring and Imaging,Motorcycle,Non-LED Lighting,Personal Computing,Pharmaceutical Packaging & Drug Delivery,Photo/Video Camera,Photovoltaic Components,Power Boat,Power Manangement,Pump,Rail Cabin Interiors,Respiratory,Scooter/Moped,Security/Detection,Semiconductor,Small Appliance,Storage/Table,Surgical Devices,Swimming Pool/Spa,Thermoplastic,Traffic Management,Trim,Vacuum Cleaner,Vending Machine,Washing Machine,Watch/Jewelry,Water Treatment/Filtration,Weaving Machine,Wireless Communications,Wiring Devices,Irrigation

Fillers

20% Glass Fiber

Processing methods

Drying Temperature: 120°C, Drying Time: 2-4hrs, Maximum Moisture Content: 0.02%, Melt Temperature: 290-320°C, Nozzle Temperature: 280-310°C, Front - Zone 3 Temperature: 290-320°C, Middle - Zone 2 Temperature: 280-310°C, Rear - Zone 1 Temperature: 270-300°C, Hopper Temperature: 60-80°C, Mold Temperature: 80-120°C