SABIC® PP 413MNK45

Want to keep this datasheet? Save it now in your required format

Description

SABIC® PP 413MNK45 is a controlled rheology PP grade with a very high fluidity. It is provided with an antistatic and nucleating agent package. This grade has a good impact – stiffness balance.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Mechanical

PropertyTemperatureValueComment

Flexural modulus

23.0 °C

1.55 GPa

Show Material materials with Flexural modulus of 1.55 GPa

ASTM D790 A

Hardness, Rockwell L

23.0 °C

94 [-]

Show Material materials with Hardness, Rockwell L of 94 [-]

ASTM D785

Thermal

PropertyValueComment

Vicat softening temperature

150 °C

Show Material materials with Vicat softening temperature of 150 °C

ASTM D1525

Technological properties

Property
Application areas

Houseware & appliances