SABIC® PP 506P

Want to keep this datasheet? Save it now in your required format

Description

SABIC® PP 506P is intended for producing low denier stretched tapes with the following features: Consistent processability; Good process ability at high line speeds and low deniers; Low tapes shrinkage; Low water carry over; Very good mechanical properties.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Mechanical

PropertyTemperatureValueComment

Flexural modulus

23.0 °C

1.5 GPa

Show Material materials with Flexural modulus of 1.5 GPa

ASTM D790 A

Hardness, Rockwell L

23.0 °C

100 [-]

Show Material materials with Hardness, Rockwell L of 100 [-]

ASTM D785

Thermal

PropertyValueComment

Vicat softening temperature

155 °C

Show Material materials with Vicat softening temperature of 155 °C

ASTM D1525

Technological properties

Property
Application areas

Carpet/Mattress/Upholstery