SABIC® PP 511A

Want to keep this datasheet? Save it now in your required format

Description

SABIC® PP 511A is a polypropylene homopolymer resin specifically designed for extrusion applications like spun bond and continuous filament spinning resulting in excellent non woven tensile properties.The narrow molecular weight distribution of SABIC® PP 511A is obtained by balanced controlled rheology. SABIC® PP 511A is compatible with all existing spun bond/continuous filament machine technologies producing different non woven compositions, produced with narrow distributed molecular weight polypropylene resins. SABIC® PP 511A has a special developed anti gas fading formulation to minimise discolouration of the fibers.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Mechanical

PropertyTemperatureValueComment

Flexural modulus

23.0 °C

1.52 GPa

Show Material materials with Flexural modulus of 1.52 GPa

ASTM D790 A

Hardness, Rockwell L

23.0 °C

104 [-]

Show Material materials with Hardness, Rockwell L of 104 [-]

ASTM D785

Thermal

PropertyValueComment

Vicat softening temperature

155 °C

Show Material materials with Vicat softening temperature of 155 °C

ASTM D1525

Technological properties

Property
Application areas

Fibers