SABIC® PP 512MK46

Want to keep this datasheet? Save it now in your required format

Description

SABIC® PP 512MK46 is specially developed for producing injection molded articles. This grade contains nucleating and antistatic agents. It has high flow properties in combination with excellent impact / stiffness balance and excellent organoleptic properties. SABIC® PP 512MK46 encompasses the following features: High top load strength & down gauging potential; Very good impact resistance; Excellent isotropic shrinkage performance (dimensional stability); High crystallization temperature and excellent flow behavior (lower cycle time); Clean product in combination of low / no odor & taste.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Mechanical

PropertyTemperatureValueComment

Elongation at yield

23.0 °C

5 %

Show Material materials with Elongation at yield of 5 %

ASTM D638

Flexural modulus

23.0 °C

1.33 GPa

Show Material materials with Flexural modulus of 1.33 GPa

ASTM D790 A

Hardness, Rockwell L

23.0 °C

98 [-]

Show Material materials with Hardness, Rockwell L of 98 [-]

ASTM D785

Yield strength

23.0 °C

27 MPa

Show Material materials with Yield strength of 27 MPa

ASTM D638

Thermal

PropertyValueComment

Vicat softening temperature

149 °C

Show Material materials with Vicat softening temperature of 149 °C

ASTM D1525

Technological properties

Property
Application areas

Multi purpose injection moulding