Description

SABIC® PP 513MK46 is specially developed for producing injection molded articles. This grade contains nucleating & antistatic agents. It has very high flow properties in combination with excellent impact / stiffness balance and excellent organoleptic properties. SABIC® PP 513MK46 encompasses the following features: High top load strength & down gauging potential Very good Impact resistance Excellent isotropy shrinkage performance (dimensional stability) High crystallization temperature and superior flow behavior (lower cycle time) Easy mold filing for aesthetic & large items Clean product in combination of low / no odor & taste

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

0.9 g/cm³

Show Material materials with Density of 0.9 g/cm³

ASTM D1505

Mechanical

PropertyTemperatureValueComment

Elongation at yield

23.0 °C

4.5 %

Show Material materials with Elongation at yield of 4.5 %

ISO 527-1/-2

Flexural modulus

23.0 °C

1.35 GPa

Show Material materials with Flexural modulus of 1.35 GPa

ASTM D790 A

Hardness, Rockwell L

23.0 °C

98 [-]

Show Material materials with Hardness, Rockwell L of 98 [-]

ASTM D785

Impact strength, Izod notched, ASTM

-20.0 °C

32 J/m

Show Material materials with Impact strength, Izod notched, ASTM of 32 J/m

ASTM D256

23.0 °C

53 J/m

Show Material materials with Impact strength, Izod notched, ASTM of 53 J/m

ASTM D256

Yield strength

23.0 °C

26 MPa

Show Material materials with Yield strength of 26 MPa

ASTM D638

Thermal

PropertyValueComment

Heat deflection temperature, 0.45 MPa

111 °C

Show Material materials with Heat deflection temperature, 0.45 MPa of 111 °C

ASTM D648

Vicat softening temperature

149 °C

Show Material materials with Vicat softening temperature of 149 °C

ASTM D1525

Technological properties

Property
Application areas

Thin wall packaging