SABIC® PP 513MN40

Want to keep this datasheet? Save it now in your required format

Description

SABIC® PP 513MN40 is a controlled rheology PP grade with very high fluidity. It contains an antistatic agent and especially developed for producing injection molded articles. This grade has a good impact resistance even at low temperature.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Mechanical

PropertyTemperatureValueComment

Flexural modulus

23.0 °C

1.2 GPa

Show Material materials with Flexural modulus of 1.2 GPa

ASTM D790 A

Hardness, Rockwell L

23.0 °C

94 [-]

Show Material materials with Hardness, Rockwell L of 94 [-]

ASTM D785

Thermal

PropertyValueComment

Vicat softening temperature

150 °C

Show Material materials with Vicat softening temperature of 150 °C

ASTM D1525

Technological properties

Property