SABIC® LLDPE 518N

Want to keep this datasheet? Save it now in your required format

Description

SABIC® LLDPE 518N is a butene linear low density polyethylene resin. Films produced from this resin have high toughness,good puncture resistance, good heat sealing behaviour and excellent machinability on conversion lines. Typical applications for SABIC® LLDPE518N are heavy duty shipping sacks, ice bags, frozen food bags, potato bags and agriculture films. Film properties: Film of 50 µm and BUR=2 has been produced on Kiefel IBC with 130 kg/h. Die size 200 mm, die gap 2,7 mm. This product is not intended for and must not be used in any pharmaceutical/medical applications.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

0.92 g/cm³

Show Material materials with Density of 0.92 g/cm³

ASTM D1505

Mechanical

PropertyTemperatureValueComment

Tear strength

23.0 °C

30 kN/m

Show Material materials with Tear strength of 30 kN/m

ISO 6383-2

Tear strength, transverse

23.0 °C

180 kN/m

Show Material materials with Tear strength, transverse of 180 kN/m

ISO 6383-2

Optical

PropertyValueComment

Haze

13 %

Show Material materials with Haze of 13 %

ASTM D1003

Technological properties

Property
Application areas

Its is used for heavy duty shipping sacks, ice bags, frozen food bags, potato bags and agriculture films.