SABIC® PP 519A

Want to keep this datasheet? Save it now in your required format

Description

SABIC® PP 519A is a polypropylene homopolymer resin specifically designed to enable optimised production speed of very fine filament titre resulting in an excellent balance of mechanical properties and softness. The rheological performance of SABIC® PP519A is providing the potential to optimise production efficiency especially for fibre production characterised by consistent high speed and low non wovens weights at reduced temperatures. SABIC® PP 519A has a very narrow molecular weight distribution. SABIC® PP 519A is compatible with all existing spun bond machine technologies producing different non woven compositions. SABIC® PP 519A has a special developed anti gas fading formulation to minimise discolouration of the fibers.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Mechanical

PropertyTemperatureValueComment

Flexural modulus

23.0 °C

1.5 GPa

Show Material materials with Flexural modulus of 1.5 GPa

ASTM D790 A

Hardness, Rockwell L

23.0 °C

102 [-]

Show Material materials with Hardness, Rockwell L of 102 [-]

ASTM D785

Thermal

PropertyValueComment

Vicat softening temperature

154 °C

Show Material materials with Vicat softening temperature of 154 °C

ASTM D1525