SABIC® PP 523P

Want to keep this datasheet? Save it now in your required format

Description

SABIC® PP 523P is a non-formulated grade, specially developed for bi-axially oriented PP (BOPP) film extrusion with a very specific molecular structure providing ultimate properties required for the stenter film process. SABIC® PP 523P is suitable for metalizable film, both as monolayer and in co-extruded structures. Films produced using SABIC® PP 523P will exhibit: Consistent processability; Very good film profile; Excellent optical properties; High tensile properties; Low residual ash; Film produced can be metalized.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Mechanical

PropertyTemperatureValueComment

Flexural modulus

23.0 °C

1.5 GPa

Show Material materials with Flexural modulus of 1.5 GPa

ASTM D790 A

Hardness, Rockwell L

23.0 °C

105 [-]

Show Material materials with Hardness, Rockwell L of 105 [-]

ASTM D785

Thermal

PropertyValueComment

Vicat softening temperature

156 °C

Show Material materials with Vicat softening temperature of 156 °C

ASTM D1525

Technological properties

Property
Application areas

It is typically used for metalizable film, both as monolayer and in co-extruded structures.