Description

SABIC® PP 526P is specially developed for cast film applications for producing clear films and do not contain slip and antiblock additives. Films produced using SABIC® PP 526P will exhibit: Consistent processability; High gloss and clarity; Good melt strength; Good mechanical properties; Film produced can be metalized.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Mechanical

PropertyTemperatureValueComment

Flexural modulus

23.0 °C

1.65 GPa

Show Material materials with Flexural modulus of 1.65 GPa

ASTM D790 A

Hardness, Rockwell L

23.0 °C

102 [-]

Show Material materials with Hardness, Rockwell L of 102 [-]

ASTM D785

Thermal

PropertyValueComment

Vicat softening temperature

152 °C

Show Material materials with Vicat softening temperature of 152 °C

ASTM D1525

Technological properties

Property
Application areas

Cast PP film