SABIC® PP5271K is a high crystallinity polypropylene homopolymer grade specifically developed for in-line and off-line thermoforming applications. SABIC® PP 5271K encompasses the following features: very high stiffness, very good clarity, very high heat distortion temperature, very good dimensional stability, good processability and fast molding cycle.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Mechanical

PropertyTemperatureValueComment

Elongation at yield

23.0 °C

8 %

Show Material materials with Elongation at yield of 8 %

ASTM D638

Flexural modulus

23.0 °C

2 GPa

Show Material materials with Flexural modulus of 2 GPa

ASTM D790 A

Hardness, Rockwell L

23.0 °C

103 [-]

Show Material materials with Hardness, Rockwell L of 103 [-]

ASTM D785

Impact strength, Izod notched, ASTM

23.0 °C

30 J/m

Show Material materials with Impact strength, Izod notched, ASTM of 30 J/m

ASTM D256

Yield strength

23.0 °C

38 MPa

Show Material materials with Yield strength of 38 MPa

ASTM D638

Thermal

PropertyValueComment

Heat deflection temperature, 0.45 MPa

120 °C

Show Material materials with Heat deflection temperature, 0.45 MPa of 120 °C

ASTM D648

Vicat softening temperature

155 °C

Show Material materials with Vicat softening temperature of 155 °C

ASTM D1525

Optical

PropertyValueComment

Haze

17 %

Show Material materials with Haze of 17 %

ASTM D 1003

Technological properties

Property
Application areas

Sheet