SABIC® Vestolen A 5640C 10000 Black

Want to keep this datasheet? Save it now in your required format

Description

SABIC® Vestolen A 5640C 10000 is a grade which has a high density and a bimodal distribution of the molecular mass. It offers a good processability and high stress cracking resistance (ESCR). SABIC® Vestolen A 5640C 10000 is typically used for the coating of steel pipes as part of a three-layer PE system. The product is not intended for and must not be used in any pharmaceutical/medical application.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

0.96 g/cm³

Show Material materials with Density of 0.96 g/cm³

ISO 1183

Mechanical

PropertyTemperatureValueComment

Hardness, Shore D

23.0 °C

57 [-]

Show Material materials with Hardness, Shore D of 57 [-]

ISO 868

Technological properties

Property
Application areas

It is typically used for the coating of steel pipes as part of a three-layer PE system.

Color

Black