SABIC® PP 56M65

Want to keep this datasheet? Save it now in your required format

Description

SABIC® PP 56M65 is specially developed for producing injection molded articles requiring a good resistance to long term heat exposure. This grade contains high heat stabilizer additive & has good heat aging resistance and good impact - stiffness balance.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Mechanical

PropertyTemperatureValueComment

Flexural modulus

23.0 °C

1.15 GPa

Show Material materials with Flexural modulus of 1.15 GPa

ASTM D790 A

Hardness, Rockwell L

23.0 °C

85 [-]

Show Material materials with Hardness, Rockwell L of 85 [-]

ASTM D785

Thermal

PropertyValueComment

Vicat softening temperature

150 °C

Show Material materials with Vicat softening temperature of 150 °C

ASTM D1525

Technological properties

Property
Application areas

Containers & pails