SABIC® PP 5702P

Want to keep this datasheet? Save it now in your required format

Description

SABIC® PP 5702P is specially developed for injection molded articles for general purpose applications. It gives consistent process ability and high gloss at the products.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Mechanical

PropertyTemperatureValueComment

Flexural modulus

23.0 °C

1.55 GPa

Show Material materials with Flexural modulus of 1.55 GPa

ASTM D790 A

Hardness, Rockwell L

23.0 °C

102 [-]

Show Material materials with Hardness, Rockwell L of 102 [-]

ASTM D785

Thermal

PropertyValueComment

Vicat softening temperature

154 °C

Show Material materials with Vicat softening temperature of 154 °C

ASTM D1525

Technological properties

Property
Application areas

Furniture