SABIC® PP 5707N

Want to keep this datasheet? Save it now in your required format

Description

SABIC® PP 5707N is a PP homopolymer grade with antistatic and nucleated agents. It is suitable for producing injection molded applications with good flow properties, good dimensional stability, high stiffness and good clarity comparing to the regular PP homopolymer grades.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Mechanical

PropertyTemperatureValueComment

Flexural modulus

23.0 °C

1.7 GPa

Show Material materials with Flexural modulus of 1.7 GPa

ASTM D790 A

Hardness, Rockwell L

23.0 °C

95 [-]

Show Material materials with Hardness, Rockwell L of 95 [-]

ASTM D785

Thermal

PropertyValueComment

Vicat softening temperature

150 °C

Show Material materials with Vicat softening temperature of 150 °C

ASTM D1525

Technological properties

Property
Application areas

Thin wall packaging