SABIC® PP 575P

Want to keep this datasheet? Save it now in your required format

Description

SABIC® PP 575P is specially developed for producing rigid injection molding articles for general purpose applications. It gives consistent processability and high gloss in the products.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

0.91 g/cm³

Show Material materials with Density of 0.91 g/cm³

ASTM D1505

Mechanical

PropertyTemperatureValueComment

Flexural modulus

23.0 °C

1.6 GPa

Show Material materials with Flexural modulus of 1.6 GPa

ASTM D790 A

Hardness, Rockwell L

23.0 °C

104 [-]

Show Material materials with Hardness, Rockwell L of 104 [-]

ASTM D785

Impact strength, Izod notched, ASTM

23.0 °C

22 J/m

Show Material materials with Impact strength, Izod notched, ASTM of 22 J/m

ASTM D256

Thermal

PropertyValueComment

Heat deflection temperature, 0.45 MPa

98 °C

Show Material materials with Heat deflection temperature, 0.45 MPa of 98 °C

ASTM D648

Vicat softening temperature

153 °C

Show Material materials with Vicat softening temperature of 153 °C

ASTM D1525

Technological properties

Property
Application areas

Multi purpose injection moulding,Furniture