SABIC® PP 5770N is a PP homopolymer grade with antistatic and nucleating agents. It is suitable for producing injection molded applications with outstanding flow properties, good dimensional stability, high stiffness, excellent organoleptic properties and good clarity comparing to the regular PP homopolymer grades. SABIC® PP 5770N encompasses the following features: very high top load strength & down gauging potential; isotropy shrinkage performance (dimensional stability); high crystallization temperature and superior flow behavior (lower cycle time); easy mold filing for aesthetic & large items; clean product in combination of low / no odor & taste.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Mechanical

PropertyTemperatureValueComment

Elongation at yield

23.0 °C

7 %

Show Material materials with Elongation at yield of 7 %

ASTM D638

Flexural modulus

23.0 °C

1.68 GPa

Show Material materials with Flexural modulus of 1.68 GPa

ASTM D790 A

Hardness, Rockwell L

23.0 °C

98 [-]

Show Material materials with Hardness, Rockwell L of 98 [-]

ASTM D785

Yield strength

23.0 °C

40 MPa

Show Material materials with Yield strength of 40 MPa

ASTM D638

Thermal

PropertyValueComment

Vicat softening temperature

150 °C

Show Material materials with Vicat softening temperature of 150 °C

ASTM D1525

Technological properties

Property
Application areas

Houseware & appliances