SABIC® PP 5780P

Want to keep this datasheet? Save it now in your required format

Description

SABIC® PP 5780P is a PP homopolymer grade with narrow molecular weight distribution and formulated with slip agent. This grade is suitable for injection molding applications require good flow properties, low COF and good gloss.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Mechanical

PropertyTemperatureValueComment

Flexural modulus

23.0 °C

1.5 GPa

Show Material materials with Flexural modulus of 1.5 GPa

ASTM D790 A

Hardness, Rockwell L

23.0 °C

104 [-]

Show Material materials with Hardness, Rockwell L of 104 [-]

ASTM D785

Thermal

PropertyValueComment

Vicat softening temperature

153 °C

Show Material materials with Vicat softening temperature of 153 °C

ASTM D1525

Technological properties

Property
Application areas

Thin wall packaging