SABIC® PP 579S

Want to keep this datasheet? Save it now in your required format

Description

SABIC® PP 579S is a PP grade with narrow molecular weight distribution. This grade is formulated with antistatic and nucleating agents. It is typically used by our customers for producing thin-walled injection molding articles and it gives low warpage tendency, high stiffness & outstanding flow properties for excellent part filling.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

0.91 g/cm³

Show Material materials with Density of 0.91 g/cm³

ASTM D1505

Mechanical

PropertyTemperatureValueComment

Flexural modulus

23.0 °C

1.9 GPa

Show Material materials with Flexural modulus of 1.9 GPa

ASTM D790 A

Hardness, Rockwell L

23.0 °C

104 [-]

Show Material materials with Hardness, Rockwell L of 104 [-]

ASTM D785

Impact strength, Izod notched, ASTM

23.0 °C

20 J/m

Show Material materials with Impact strength, Izod notched, ASTM of 20 J/m

ASTM D256

Thermal

PropertyValueComment

Heat deflection temperature, 0.45 MPa

98 °C

Show Material materials with Heat deflection temperature, 0.45 MPa of 98 °C

ASTM D648

Vicat softening temperature

152 °C

Show Material materials with Vicat softening temperature of 152 °C

ASTM D1525

Technological properties

Property
Application areas

Thin wall packaging,Houseware & appliances