SABIC® PP 57MNK40

Want to keep this datasheet? Save it now in your required format

Description

SABIC® PP 57MNK40 is a controlled rheology PP grade and specially developed for producing injection molded articles. This grade contains nucleating & antistatic agents. It has excellent impact resistance (even at low temperature) and balanced stiffness.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Mechanical

PropertyTemperatureValueComment

Flexural modulus

23.0 °C

1.15 GPa

Show Material materials with Flexural modulus of 1.15 GPa

ASTM D790 A

Hardness, Rockwell L

23.0 °C

80 [-]

Show Material materials with Hardness, Rockwell L of 80 [-]

ASTM D785

Impact strength, Izod notched, ASTM

-20.0 °C

63 J/m

Show Material materials with Impact strength, Izod notched, ASTM of 63 J/m

ASTM D256

23.0 °C

115 J/m

Show Material materials with Impact strength, Izod notched, ASTM of 115 J/m

ASTM D256

Thermal

PropertyValueComment

Heat deflection temperature, 0.45 MPa

90 °C

Show Material materials with Heat deflection temperature, 0.45 MPa of 90 °C

ASTM D648

Vicat softening temperature

148 °C

Show Material materials with Vicat softening temperature of 148 °C

ASTM D1525

Technological properties

Property
Application areas

Houseware & appliances