SABIC® PP 595A has been specially developed for use in automotive compounding. The material has high flow properties and a high stiffness, enabling high production rates. It is formulated with a dedicated automotive additive package.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

0.91 g/cm³

Show Material materials with Density of 0.91 g/cm³

ASTM D1505

Mechanical

PropertyTemperatureValueComment

Elongation at yield

23.0 °C

11 %

Show Material materials with Elongation at yield of 11 %

ISO 527-1/-2

Flexural modulus

23.0 °C

1.8 GPa

Show Material materials with Flexural modulus of 1.8 GPa

ASTM D790 A

Hardness, Rockwell L

23.0 °C

104 [-]

Show Material materials with Hardness, Rockwell L of 104 [-]

ASTM D785

Impact strength, Izod notched, ASTM

23.0 °C

20 J/m

Show Material materials with Impact strength, Izod notched, ASTM of 20 J/m

ASTM D256

Yield strength

23.0 °C

35 MPa

Show Material materials with Yield strength of 35 MPa

ASTM D638

Thermal

PropertyValueComment

Heat deflection temperature, 0.45 MPa

108 °C

Show Material materials with Heat deflection temperature, 0.45 MPa of 108 °C

ASTM D648

Vicat softening temperature

152 °C

Show Material materials with Vicat softening temperature of 152 °C