SABIC® LLDPE 6118LE

Want to keep this datasheet? Save it now in your required format

Description

SABIC® LLDPE 6118LE is a hexene linear low density polyethylene resin. Films made from this resin exhibitgood tensile strength, stiffness, dart drop impact strength, tear strength and hottack properties. This resincontains anti block and slip agent. Application Typical application for SABIC® LLDPE 6118LE are heavy duty bags, lamination films, agriculture films, stretchwrap films, frozen food packaging and other applications requiring high impact strength, high tear resistance and improved sealing properties. Film properties Film of 50 μm and BUR = 2 has been produced on Kiefel IBC with 140 kg/h. Die size 200 mm, die gap 2.7 mm. This product is not intended for and must not be used in any pharmaceutical/medical applications.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Coefficient of friction

0.1 [-]

Show Material materials with Coefficient of friction of 0.1 [-]

ASTM D1894

Density

23.0 °C

0.92 g/cm³

Show Material materials with Density of 0.92 g/cm³

ASTM D1505

Mechanical

PropertyTemperatureValueComment

Tear strength

23.0 °C

100 kN/m

Show Material materials with Tear strength of 100 kN/m

ISO 6383-2

Tear strength, transverse

23.0 °C

400 kN/m

Show Material materials with Tear strength, transverse of 400 kN/m

ISO 6383-2

Optical

PropertyValueComment

Haze

13 %

Show Material materials with Haze of 13 %

ASTM D1003

Technological properties

Property
Application areas

Heavy duty bags, lamination films, agriculture films, stretchwrap films, frozen food packaging and other applications requiring high impact strength, high tear resistance and improved sealing properties.