SABIC® LLDPE 6218B

Want to keep this datasheet? Save it now in your required format

Description

SABIC® LLDPE 6218Bis a hexene-linear low density polyethylene. ApplicationTypical application for SABIC® LLDPE6218B Film propertiesFilm of 50 µm with BUR=2 is produced on Kiefel IBC with 140 kg/h. Die size 200 mm, die gap 1.8 mm.The product mentioned herein is in particular not tested and therefore not validated for use in pharmaceutical/ medical applications.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

0.92 g/cm³

Show Material materials with Density of 0.92 g/cm³

ASTM D1505

Mechanical

PropertyTemperatureValueComment

Tear strength

23.0 °C

80 kN/m

Show Material materials with Tear strength of 80 kN/m

ISO 6383-2

Tear strength, transverse

23.0 °C

260 kN/m

Show Material materials with Tear strength, transverse of 260 kN/m

ISO 6383-2

Optical

PropertyValueComment

Haze

35 %

Show Material materials with Haze of 35 %

ASTM D1003

Technological properties

Property
Application areas

Stretch film,General purpose film,Heavy duty film,Cast film