SABIC® LLDPE 6318B

Want to keep this datasheet? Save it now in your required format

Description

6318BJ resin is a hexene comonomer based Linear Low Density Polyethylene TNPP free grade designed to provide easy processability and specially formulated for optimum thermal stability at high processing temperatures used during production of Cast films. Films produced using this resin gives excellent optical properties, toughness, puncture resistance and tear strength.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

0.92 g/cm³

Show Material materials with Density of 0.92 g/cm³

ASTM D1505

Mechanical

PropertyTemperatureValueComment

Tear strength

23.0 °C

1960 kN/m

Show Material materials with Tear strength of 1960 kN/m

ASTM D1922

Tear strength, transverse

23.0 °C

7840 kN/m

Show Material materials with Tear strength, transverse of 7840 kN/m

ASTM D1922

Optical

PropertyValueComment

Haze

1.7 %

Show Material materials with Haze of 1.7 %

ASTM D1003

Technological properties

Property
Application areas

Stretch film