SABIC® LLDPE 6318BE

Want to keep this datasheet? Save it now in your required format

Description

SABIC® LLDPE 6318BE is a hexene linear low density polyethylene resin for cast film applications. The product is typically formulated for optimum thermal stability at high temperatures used in cast film extrusion. Films produced from this grade exhibit good optical properties, toughness, puncture resistance and tear strength. Application SABIC® LLDPE 6318BE resin is typically used for pallet stretch wrap (pre-stretch), high performance draw down films and other mono layer and coextruded film applications where high strength is required. The grade is also suggested for blending with ethylene/butene copolymer LLDPE and LDPE for improving strength. Film properties Properties are determined on 20 μm cast stretch film produced on a 2 m commercial cast stretch line: melt temperature 270 °C, chill roll temperature 20 °C and line speed 450 m/min. Processing conditions SABIC® LLDPE 6318BE is extrudable with conventional cast film extrusion equipment. Temperatures 250- 300°C. This product is not intended for and must not be used in any pharmaceutical/medical applications.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

0.92 g/cm³

Show Material materials with Density of 0.92 g/cm³

ASTM D1505

Mechanical

PropertyTemperatureValueComment

Tear strength, transverse

23.0 °C

246 kN/m

Show Material materials with Tear strength, transverse of 246 kN/m

ISO 6383-2

Optical

PropertyValueComment

Haze

1.8 %

Show Material materials with Haze of 1.8 %

ASTM D1003

Technological properties

Property
Application areas

It is typically used for pallet stretch wrap (pre-stretch), high performance draw down films and other mono layer and coextruded film applications where high strength is required.