SABIC® PP 642NH-66408

Want to keep this datasheet? Save it now in your required format

Description

SABIC® PP 642NH-66408 is a high molecular weight, low melt flow rate polypropylene random copolymer (PP-R) green coloured and specially designed for transport of hot and cold drinking water. This grade is highly heat stabilized and specially formulated for extraction resistance with improved throughput & gloss.SABIC®PP 642NH-66408 is pre-color compounded version of SABIC®PP 651H PPR resin (Exova – MRS classification 8 MPa). SABIC®PP 642NH-66408 is a designated pipe grade.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

0.9 g/cm³

Show Material materials with Density of 0.9 g/cm³

ASTM D1505

Mechanical

PropertyTemperatureValueComment

Flexural modulus

23.0 °C

1.04 GPa

Show Material materials with Flexural modulus of 1.04 GPa

ISO 178

Technological properties

Property
Application areas

Specially designed for transport of hot and cold drinking water.