SABIC® LLDPE 6821NJ

Want to keep this datasheet? Save it now in your required format

Description

6821NJ is a fractional melt index hexene copolymer based Linear Low Density Polyethylene TNPP free grade suitable for high strength packaging applications. Films produced using this resin gives outstanding toughness, excellent puncture resistance, good sealing characteristics and tear resistance. 6821NJ contains no slip and no antiblock additive.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

0.92 g/cm³

Show Material materials with Density of 0.92 g/cm³

ASTM D1505

Thermal

PropertyValueComment

Vicat softening temperature

101 °C

Show Material materials with Vicat softening temperature of 101 °C

ASTM D1525

Optical

PropertyValueComment

Haze

12 %

Show Material materials with Haze of 12 %

ASTM D1003

Technological properties

Property
Application areas

It is used for high strength packaging applications