SABIC® SUPEER™ 7118NE

Want to keep this datasheet? Save it now in your required format

Description

SABIC® SUPEER™ 7118NE is a metallocene ethylene-hexene copolymer. It has a good processability and performs well in a wide range of general purpose and high performance blown film applications. Films produced with this grade offer good tensile and impact strength, puncture resistance and sealing properties. SABIC® SUPEER™ 7118NE is typically used for applications like heavy duty bags, agriculture film, stretch hood, lamination film, frozen bags. Properties have been measured on blown film of 25 µm and BUR = 2.5 Typical processing conditions for SABIC® SUPEER™ 7118NE : processing temperatures 180 - 230 °C Blow up ratio: 2.0 - 4.0 This product is not intended for and must not be used in any pharmaceutical/medical applications.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Mechanical

PropertyTemperatureValueComment

Tear strength

23.0 °C

117.6 kN/m

Show Material materials with Tear strength of 117.6 kN/m

ASTM D1922

Tear strength, transverse

23.0 °C

176.4 kN/m

Show Material materials with Tear strength, transverse of 176.4 kN/m

ASTM D1922

Optical

PropertyValueComment

Haze

20 %

Show Material materials with Haze of 20 %

ASTM D1003

Technological properties

Property
Application areas

Heavy duty bags, agriculture film, stretch hood, lamination film, frozen bags.