SABIC® LLDPE 726QE

Want to keep this datasheet? Save it now in your required format

Description

SABIC® LLDPE 726QE is a butene linear low density polyethylene resin. This grade gives blown films a relatively high stiffness for good machinability and a good overall balance of other performance properties, such as puncture resistance, impact strength and heat sealability. This material contains anti block, slip agent and processing aid. Application Typical applications for SABIC® LLDPE 726QE are shipping sacks, produce bags, can liners and carrier bags. SABIC® LLDPE 726QE has very good optical properties when blended with a LDPE (15-85%). Film properties Film of 50 μm and BUR=2 has been produced on Kiefel IBC with 130 kg/h. Die size 200 mm, die gap 0.8 mm. This product is not intended for and must not be used in any pharmaceutical/medical applications.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Coefficient of friction

0.1 [-]

Show Material materials with Coefficient of friction of 0.1 [-]

ASTM D1894

Density

23.0 °C

0.93 g/cm³

Show Material materials with Density of 0.93 g/cm³

ASTM D1505

Mechanical

PropertyTemperatureValueComment

Tear strength

23.0 °C

23 kN/m

Show Material materials with Tear strength of 23 kN/m

ISO 6383-2

Tear strength, transverse

23.0 °C

130 kN/m

Show Material materials with Tear strength, transverse of 130 kN/m

ISO 6383-2

Optical

PropertyValueComment

Haze

14 %

Show Material materials with Haze of 14 %

ASTM D1003

Technological properties

Property
Application areas

Shipping sacks, produce bags, can liners and carrier bags.