SABIC® SUPEER™ 8118L

Want to keep this datasheet? Save it now in your required format

Description

SABIC® SUPEER™ 8118L is an ethylene-octene copolymer produced via solution polymerization using metallocene catalyst. It performs well in a wide range of general purpose and high performance LLDPE blown film applications and have excellent processability. It contains slip and antiblock additives.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

0.92 g/cm³

Show Material materials with Density of 0.92 g/cm³

ASTM D1505

Thermal

PropertyValueComment

Melting point

115 °C

Show Material materials with Melting point of 115 °C

SABIC method

Optical

PropertyValueComment

Haze

10 %

Show Material materials with Haze of 10 %

ASTM D1003

Technological properties

Property
Application areas

Stretch film,Lamination film,Heavy duty film