SABIC® COHERE™ 8170D

Want to keep this datasheet? Save it now in your required format

Description

SABIC® COHERE™ 8170D is an ethylene-octene copolymer produced via solution polymerization using metallocene catalyst. It can be used in monolayer or coextruded film to enhance heat-sealing properties, clarity, toughness, flexibility and elasticity. It has strict gel control to meet high quality film requirements.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Mechanical

PropertyTemperatureValueComment

Flexural modulus

23.0 °C

13.2 GPa

Show Material materials with Flexural modulus of 13.2 GPa

ASTM D790 A

Tear strength

23.0 °C

39.2 kN/m

Show Material materials with Tear strength of 39.2 kN/m

ASTM D624

Thermal

PropertyValueComment

Melting point

62 °C

Show Material materials with Melting point of 62 °C

SABIC method

Technological properties

Property
Application areas

Blown film