SABIC® PP 85M10T

Want to keep this datasheet? Save it now in your required format

Description

SABIC® PP 85M10T is a low fluidity polypropylene impact copolymer with good processability, very high impact strength and medium stiffness. It contains antistatic agents.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

0.91 g/cm³

Show Material materials with Density of 0.91 g/cm³

ISO 1183

Mechanical

PropertyTemperatureValueComment

Flexural modulus

23.0 °C

1.05 GPa

Show Material materials with Flexural modulus of 1.05 GPa

ASTM D790 A

Yield strength

23.0 °C

23 MPa

Show Material materials with Yield strength of 23 MPa

ASTM D638

Technological properties

Property
Application areas

Houseware & appliances,Containers & pails