SABIC® POM 90S

Want to keep this datasheet? Save it now in your required format

Description

SABIC® POM 90S is a medium molecular weight grade suitable for Injection molding applications for parts requiring high rigidity and strength for many applications.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.41 g/cm³

Show Material materials with Density of 1.41 g/cm³

ISO 1183

Water absorption

23.0 °C

0.65 %

Show Material materials with Water absorption of 0.65 %

ISO 62

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

2.85 GPa

Show Material materials with Elastic modulus of 2.85 GPa

ISO 527-2 1A | 1mm/min

Elongation at yield

23.0 °C

9 %

Show Material materials with Elongation at yield of 9 %

ISO 527-2 1A | 50mm/min

Flexural modulus

23.0 °C

2.7 GPa

Show Material materials with Flexural modulus of 2.7 GPa

ISO 178

Impact strength, Charpy notched

-30.0 °C

160 kJ/m²

Show Material materials with Impact strength, Charpy notched of 160 kJ/m²

ISO 179/1eU

23.0 °C

180 kJ/m²

Show Material materials with Impact strength, Charpy notched of 180 kJ/m²

ISO 179/1eU

Yield strength

23.0 °C

64 MPa

Show Material materials with Yield strength of 64 MPa

ISO 527-2 1A | 50 mm/min

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

1.1E-4 1/K

Show Material materials with Coefficient of thermal expansion of 1.1E-4 1/K

ISO 11359-2

Heat deflection temperature, 1.80 MPa

104 °C

Show Material materials with Heat deflection temperature, 1.80 MPa of 104 °C

ISO 75-1&2 | 1.8 MPa

Melting point

166 °C

Show Material materials with Melting point of 166 °C

ISO 11357-1/-3

Rheological Properties

PropertyTemperatureValueComment

Melt volume-flow rate

8 cm³/10min

Show Material materials with Melt volume-flow rate of 8 cm³/10min

ISO 1133

Shrinkage

23.0 °C

2 %

Show Material materials with Shrinkage of 2 %

ISO 294-4

Shrinkage, transverse

23.0 °C

1.8 %

Show Material materials with Shrinkage, transverse of 1.8 %

ISO 294-4